Poly(4-tert-butylcyclohexyl methacrylate)
CROW logo
Poly(4-tert-butylcyclohexyl methacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylates
COMMON NAMESPoly(4-tert-butylcyclohexyl methacrylate)
STRUCTURE BASED NAME Poly(4-tert-butylcyclohexyl 2-methylpropenoate)
ACRONYMS  
CAS # 34903-89-4
CurlySMILES C{-}C{n+}(C)(C(=O)OC1CCC(CC1)C(C)(C)C)
 

IDENTIFIERS OF MONOMER(S)

CAS # 256-277-5
COMMON NAMES4-tert-Butylcyclohexyl methacrylate, 4-(1,1-Dimethylethyl)cyclohexyl methacrylate
SMILES CC(=C)C(=O)OC1CCC(CC1)C(C)(C)C
Std. InChI 1S/C14H24O2/c1-10(2)13(15)16-12-8-6-11(7-9-12)14(3,4)5/h11-12H,1,6-9H2,2-5H3
Std. InChIKey PILKNUBLAZTESB-UHFFFAOYSA-N
STRUCTURE
tert-Butyl acrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 228
Density ρg mL-1 0.99
Solubility Parameter δMPa1/2
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 356 - 451403
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1 48400 - 5160050000
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 224.34
Van-der-Waals Volume VvWmL mol-1 141.5
Molar Volume VmmL mol-1 214 - 221217
Density ρg mL-1 1.02 - 1.051.03
Solubility Parameter δMPa1/2 17.1 - 17.717.4
Molar Cohesive Energy EcohJ mol-1 62700 - 6810065500
Glass Transition Temperature TgK 390 - 392391
Molar Heat Capacity CpJ (mol K)-1 308 -325315
Entanglement Molecular Weight Meg mol-1 45800 -  5300049400
Index of Refraction nnone 1.50 

  Last updated: September 30, 2016